Please note that eDoc will be permanently shut down in the first quarter of 2021!      Home News About Us Contact Contributors Disclaimer Privacy Policy Help FAQ

Home
Search
Quick Search
Advanced
Fulltext
Browse
Collections
Persons
My eDoc
Session History
Login
Name:
Password:
Documentation
Help
Support Wiki
Direct access to
document ID:


          Institute: Fritz-Haber-Institut     Collection: Inorganic Chemistry     Display Documents



  history
ID: 48759.0, Fritz-Haber-Institut / Inorganic Chemistry
Comparison of Tetragonal and Ordered Mesoporous Sulfated ZrO2:
Alkane Isomerization Studied by In Situ DR UV-vis Spectroscopy
Authors:Ahmad, Rafat; Melsheimer, Jörg; Yang, Xiaobo; Tzolova-Müller, Genka; Jentoft, Friederike C.
Language:English
Research Context:Project 1: Acid-base & redox properties of promoted sulfated zirconia
Name of Conference/Meeting:Europacat-VI
Place of Conference/Meeting:Innsbruck / Austria
(Start) Date of Event 
 (YYYY-MM-DD):
2003-08-31
End Date of Conference/Meeting 
 (YYYY-MM-DD):
2003-09-04
Audience:Experts Only
Abstract / Description:Introduction: The role of the ZrO2 bulk structure in sulfated zirconia (SZ) catalysts is unclear. We compare SZ of tetragonal structure (tSZ) to ordered mesoporous SZ of MCM-41 structure (omSZ), focussing on performance and deactivation behavior in n-butane and n-pentane isomerization.
Experimental: tSZ was obtained by calcination of a commercial precursor, omSZ in a procedure based on the description by Ciesla [1,2]. In situ DR-UV-vis-NIR spectra were recorded using a lambda 9 spectrometer (PerkinElmer) with integrating sphere and a fixed bed flow reactor [3]. Products of n-butane (5 kPa in He) and n-pentane (1 kPa) isomerization were analyzed by on-line GC.
Results and Discussion: tSZ exhibited a higher maximum activity than omSZ; to obtain comparable rates, conditions were varied. For n-butane isomerization catalyzed by tSZ at 378 K, the conversion increased over 50 min and then declined in the next 100 min to a steady state. Despite a higher reaction temperature of 453 K, omSZ, which passed through a 100 min induction period, deactivated only slowly. Both catalysts produced propane and pentanes as side products, suggesting a similar mode of operation. During the deactivation phase, which stretched over 100 min for tSZ and over more than 900 min for omSZ, bands developed in the UV-vis spectra. A band at 310 nm was detected for tSZ and assigned to allylic cations; for omSZ, the band was positioned at 285 nm. In the reaction with n-pentane, the materials produced more isobutane than isopentane within the observation span of 15 h. Both catalysts deactivated rapidly while bands at 330 nm (tSZ, 298 K) and 285 nm with a shoulder at ca. 330 nm (omSZ, 323 K) formed. Unsaturated species are formed on both materials but they are either differently polarized by the surface or differently structured, indicating an influence of the nature of the ZrO2 structure.
1. U. Ciesla, S. Schacht, G.D. Stucky, K.K. Unger, F. Schüth, Angew. Chem. 108 (1996) 597.
2. X. Yang, F.C. Jentoft, R.E. Jentoft, F. Girgsdies, T. Ressler, Catal. Lett. 81 (2002) 25.
3. M. Thiede, J. Melsheimer, Rev. Sci. Inst. 73 (2002) 394.
Document Type:Poster
Communicated by:Robert Schlögl
Affiliations:Fritz-Haber-Institut/Inorganic Chemistry/Functional Characterization
Full Text:
You have privileges to view the following file(s):
europacat_2003_abstract.pdf  [240,00 Kb]   
 
The scope and number of records on eDoc is subject to the collection policies defined by each institute - see "info" button in the collection browse view.